The clinical development of the glass-ionomer cement. III. The erosion lesion.
Aust Dent J, 1977/6;22(3):190-5.
PMID: 337956
Impact factor: 2.259
Abstract
A clinical trial of the glass-ionomer cement, ASPA IV, as a restorative material for erosion lesions is reported. The failure rate, in a three-year trial, was nine per cent; most failures occurring within the first few months after placement.
MeSH terms
Acrylic Resins; Dental Bonding; Dental Cavity Preparation; Dental Restoration, Permanent; Glass; Humans; Polycarboxylate Cement; Tooth Erosion